NDT Buyers Guide

Company Information:

Name:

Magnaflux

Division: 

Div. of Illinois Tool Works

Address:

3624 W. Lake Ave.
Glenview, IL 60026
UNITED STATES

Phone:

(847) 657-5300

Fax:

(800) 421-1569

(847) 657-5388

Email:

cs@magnaflux.com

kgreen@magnaflux.com

Website:

www.magnaflux.com

Company Description:

Over 80 years experience as a global manufacturer of magnetic particle, and liquid penetration inspection equipment, associated materials and accessory products used for non-destructive testing. Magnaflux offers an aqueous cleaning line, as well as a complete line of Ultrasonic Couplants.

Products:

  • Blacklight
  • Liquid Penetrant Testing, Penetrants
  • Magnetic Particle Testing, Magnetic Particles
  • Magnetic Particle Testing, Yokes
  • Ultrasonic Test Equipment, Ultrasonic Couplants