NDT Buyers Guide

Company Information:

Name:

Proceco Ltd.

Address:

7300 Tellier St.
Montreal, QC H1N 3T7
CANADA

Phone:

(800) 978-6677

(514) 254-8494

Fax:

(514) 254-6922

Email:

cleaning@proceco.com

Website:

www.proceco.com

http://proceco.com/products/liquid-penetrant/liquid-penetrant.php

Company Description:

PROCECO manufactures custom-designed, automated and semi-automated liquid penetrant inspection systems,for fluorescent penetrant (FPI) and blue etch processes for aerospace components. Penetrant systems are integrating part cleaning and back striping processes.

Products:

  • Fluorescent Inspection
  • Immersion Tanks
  • Liquid Penetrant Testing, Processing Equipment
  • Penetrant Systems
Quality Buyers Guide